{"data":[{"pos":2,"id":17252,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100 BK602","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-03-10 10:02:18","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"High Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"High Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11800,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100 NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-03-10 09:57:12","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"High Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"High Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11801,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100AF","abbt":"POM-Z20","pname":"","pshortname":"DuPont","lastchange":"2026-02-03 13:12:49","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"20% PTFE Fiber Filled High Viscosity Acetal Homopolymer with Low Wear and Low Friction"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"20% PTFE Fiber Filled High Viscosity Acetal Homopolymer with Low Wear and Low Friction"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11802,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100AL NC010","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2026-01-23 16:23:42","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":52508,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100ALE NC010","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2026-02-05 11:37:29","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":2},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction\u00a0and Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction\u00a0and Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":78614,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100CPE BK602","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-23 16:24:28","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":2},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"High Viscosity Acetal Homopolymer with Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"High Viscosity Acetal Homopolymer with Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":46069,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100CPE NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-02-05 11:33:12","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"High Viscosity Acetal Homopolymer with Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"High Viscosity Acetal Homopolymer with Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11803,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100KM NC000","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2026-01-23 16:07:46","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Kevlar\u00ae Modified High Viscosity Acetal Homopolymer with Low Wear and Low Friction"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Kevlar\u00ae Modified High Viscosity Acetal Homopolymer with Low Wear and Low Friction"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":17100,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100P BK602","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-23 16:25:04","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"High Viscosity Acetal Homopolymer with Improved Processing"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"High Viscosity Acetal Homopolymer with Improved Processing"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11804,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100P NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-02-06 10:58:55","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"High Viscosity Acetal Homopolymer with Improved Processing"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"High Viscosity Acetal Homopolymer with Improved Processing"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":17102,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100ST BK602","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-23 16:25:55","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Super Toughened High Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Super Toughened High Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11806,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100ST NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-03-10 09:57:12","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Super Toughened High Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Super Toughened High Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":17059,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100STE NC010","abbt":"POM-I","pname":"","pshortname":"DuPont","lastchange":"2026-02-05 11:09:16","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Super Toughened High Viscosity Acetal Homopolymer with Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Super Toughened High Viscosity Acetal Homopolymer with Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":17103,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100T BK602","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-23 16:30:33","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Toughened High Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Toughened High Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11807,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100T NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-02-05 14:50:53","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Toughened High Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Toughened High Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":17058,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100TE NC010","abbt":"POM-I","pname":"","pshortname":"DuPont","lastchange":"2026-02-05 15:09:15","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Toughened High Viscosity Acetal Homopolymer with Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Toughened High Viscosity Acetal Homopolymer with Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":17104,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 100TL NC010","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2026-01-23 16:33:07","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"PTFE Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"PTFE Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":58057,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 111DP BK402","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-23 16:41:08","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated High Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated High Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":26769,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 111DP NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-02-05 15:00:11","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated High Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated High Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":20484,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 111PA NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-06-03 15:47:30","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":8},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated High Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated High Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":17105,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 127UV BK701","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-23 16:48:31","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"UV Stabilised High Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"UV Stabilised High Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11813,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 127UV NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-23 16:50:53","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"UV Stabilised High Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"UV Stabilised High Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":30549,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 127UVE BK701","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-23 16:58:48","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":10},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":16448,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 127UVE NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-02-05 11:09:05","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"UV Stabilised High Viscosity Acetal Homopolymer with Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"UV Stabilised High Viscosity Acetal Homopolymer with Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11815,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 150 NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-26 08:23:44","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"High Viscosity Acetal Homopolymer Developed for Extrusion"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"High Viscosity Acetal Homopolymer Developed for Extrusion"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":78978,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 300ATB BK000","abbt":"POM-I-CD","pname":"","pshortname":"DuPont","lastchange":"2023-11-30 10:21:53","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":2},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Toughened, Static Dissipative, Medium Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Toughened, Static Dissipative, Medium Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":34249,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 300CP BK602","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-26 08:31:00","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium-high Viscosity Acetal Homopolymer with Improved Processing"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium-high Viscosity Acetal Homopolymer with Improved Processing"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11819,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 300CP NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-26 08:32:26","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium-high Viscosity Acetal Homopolymer with Improved Processing"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium-high Viscosity Acetal Homopolymer with Improved Processing"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":64617,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 300CPE NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-02-06 10:47:28","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":2},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium-high Viscosity Acetal Homopolymer with Improved Processing\u00a0and Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium-high Viscosity Acetal Homopolymer with Improved Processing\u00a0and Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":17109,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 300TE BK602","abbt":"POM-I","pname":"","pshortname":"DuPont","lastchange":"2026-01-26 08:39:15","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Toughened Medium-high Viscosity Acetal Homopolymer with Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Toughened Medium-high Viscosity Acetal Homopolymer with Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":13743,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 300TE NC010","abbt":"POM-I","pname":"","pshortname":"DuPont","lastchange":"2026-02-06 10:48:08","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Toughened Medium-high Viscosity Acetal Homopolymer with Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Toughened Medium-high Viscosity Acetal Homopolymer with Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":17110,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 311DP BK402","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-26 08:41:26","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated Medium-high Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated Medium-high Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11821,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 311DP NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-26 08:42:35","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated Medium-high Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated Medium-high Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":16449,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 327UVE NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-02-05 11:25:53","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"UV Stabilised Medium-high Viscosity Acetal Homopolymer with Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"UV Stabilised Medium-high Viscosity Acetal Homopolymer with Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11825,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 500AF","abbt":"POM-Z20","pname":"","pshortname":"DuPont","lastchange":"2025-08-18 13:59:35","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"20% PTFE Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"20% PTFE Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":11826,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 500AL NC010","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 10:58:05","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":17112,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 500CL BK601","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 11:00:14","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":11827,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 500CL NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 11:01:29","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":63685,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 500CPE BK602","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 11:02:12","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium Viscosity Acetal Homopolymer with Improved Processing\u00a0and Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium Viscosity Acetal Homopolymer with Improved Processing\u00a0and Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":58121,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 500CPE NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-02-05 15:15:58","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium Viscosity Acetal Homopolymer with Improved Processing\u00a0and Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium Viscosity Acetal Homopolymer with Improved Processing\u00a0and Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":20492,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 500MT NC010","abbt":"POM-I","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 11:04:14","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":8},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium Toughened, Toughened, Medium Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium Toughened, Toughened, Medium Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":17113,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 500P BK602","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 11:20:50","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium Viscosity Acetal Homopolymer with Improved Processing"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium Viscosity Acetal Homopolymer with Improved Processing"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":11831,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 500P NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-02-05 15:54:19","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium Viscosity Acetal Homopolymer with Improved Processing"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium Viscosity Acetal Homopolymer with Improved Processing"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":11833,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 500SC NC010","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2025-02-05 15:40:54","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Silicone Lubricated Medium Viscosity Acetal Homopolymer Concentrate Developed for Enhancing Lubricity"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Silicone Lubricated Medium Viscosity Acetal Homopolymer Concentrate Developed for Enhancing Lubricity"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":17115,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 500T BK602","abbt":"POM-I","pname":"","pshortname":"DuPont","lastchange":"2026-03-10 10:01:02","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Toughened Medium Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Toughened Medium Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":11834,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 500T NC010","abbt":"POM-I","pname":"","pshortname":"DuPont","lastchange":"2026-03-10 10:01:02","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Toughened Medium Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Toughened Medium Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":11835,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 500TL NC010","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 11:29:38","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"PTFE Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"PTFE Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":11836,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 510GR NC000","abbt":"POM-GF10","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 11:33:07","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"10% Glass Reinforced Medium Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"10% Glass Reinforced Medium Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":52489,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 511CPE NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 11:33:26","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated Medium Viscosity Acetal Homopolymer with Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated Medium Viscosity Acetal Homopolymer with Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":17116,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 511DP BK402","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 11:34:58","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated Medium Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated Medium Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11837,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 511DP NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 11:36:22","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated Medium Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated Medium Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":78843,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 51HSE NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-02-04 09:53:17","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":2},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated Very High Viscosity Acetal Homopolymer with Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated Very High Viscosity Acetal Homopolymer with Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11839,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 520MP NC010","abbt":"POM-Z20","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 11:41:17","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"20% PTFE Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"20% PTFE Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":21871,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 525GR BK000","abbt":"POM-GF25","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 14:34:31","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"25% Glass Reinforced Medium Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"25% Glass Reinforced Medium Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":26774,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 525GR NC000","abbt":"POM-GF25","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 14:35:34","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"25% Glass Reinforced Medium Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"25% Glass Reinforced Medium Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":17117,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 527UV BK701","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 14:36:21","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"UV Stabilised Medium Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"UV Stabilised Medium Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":11841,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 527UV NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 14:37:42","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"UV Stabilised Medium Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"UV Stabilised Medium Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":17118,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 527UVE RD402","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 15:13:24","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":8},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"UV Stabilised Medium Viscosity Acetal Homopolymer with Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"UV Stabilised Medium Viscosity Acetal Homopolymer with Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":17119,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 900P BK602","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 15:20:03","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Low Viscosity Acetal Homopolymer with Improved Processing"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Low Viscosity Acetal Homopolymer with Improved Processing"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":11848,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 900P NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-27 15:33:15","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Low Viscosity Acetal Homopolymer with Improved Processing"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Low Viscosity Acetal Homopolymer with Improved Processing"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":11850,"state":0,"general":{"pos":2,"name":"Delrin\u00ae 911DP NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-29 11:06:23","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated Low Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated Low Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":21939,"state":0,"general":{"pos":2,"name":"Delrin\u00ae FG100 NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-06-20 18:19:21","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":2},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"High Viscosity Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"High Viscosity Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11860,"state":0,"general":{"pos":2,"name":"Delrin\u00ae FG100AL NC010","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2026-01-29 11:49:38","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11861,"state":0,"general":{"pos":2,"name":"Delrin\u00ae FG100P NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-01-29 11:50:39","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":8},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"High Viscosity Acetal Homopolymer Developed for Food Contact Applications"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"High Viscosity Acetal Homopolymer Developed for Food Contact Applications"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11862,"state":0,"general":{"pos":2,"name":"Delrin\u00ae FG100TL NC010","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2025-02-19 15:43:36","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"PTFE Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"PTFE Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":67336,"state":0,"general":{"pos":2,"name":"Delrin\u00ae FG111DP NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-02-19 15:43:44","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated High Viscosity Acetal Homopolymer\u00a0Developed for Food Contact Applications"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated High Viscosity Acetal Homopolymer\u00a0Developed for Food Contact Applications"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11863,"state":0,"general":{"pos":2,"name":"Delrin\u00ae FG150 NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-02-19 15:43:52","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"High Viscosity Acetal Homopolymer Developed for Food Contact Applications"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"High Viscosity Acetal Homopolymer Developed for Food Contact Applications"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11864,"state":0,"general":{"pos":2,"name":"Delrin\u00ae FG311DP NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-08-18 14:00:02","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11867,"state":0,"general":{"pos":2,"name":"Delrin\u00ae FG500AL NC010","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2025-08-18 13:58:00","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":48291,"state":0,"general":{"pos":2,"name":"Delrin\u00ae FG500MXD BLA090","abbt":"POM-(MD+X)","pname":"","pshortname":"DuPont","lastchange":"2025-02-19 15:44:25","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":10},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"X-ray\u00a0and\u00a0Metal\u00a0Detectable Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"X-ray\u00a0and\u00a0Metal\u00a0Detectable Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11868,"state":0,"general":{"pos":2,"name":"Delrin\u00ae FG500P NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-08-18 14:00:07","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":11870,"state":0,"general":{"pos":2,"name":"Delrin\u00ae FG511DP NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-05-23 13:55:19","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":11871,"state":0,"general":{"pos":2,"name":"Delrin\u00ae FG900P NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-08-18 13:58:08","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Low Viscosity Acetal Homopolymer Developed for Food Contact Applications"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Low Viscosity Acetal Homopolymer Developed for Food Contact Applications"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":34275,"state":0,"general":{"pos":2,"name":"Delrin\u00ae FG911DP NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-02-19 15:45:16","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":10},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated Low Viscosity Acetal Homopolymer Developed for Food Contact Applications"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated Low Viscosity Acetal Homopolymer Developed for Food Contact Applications"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":24088,"state":0,"general":{"pos":2,"name":"Delrin\u00ae PC650 NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-02-19 15:41:43","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":8},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium Viscosity Acetal Homopolymer Developed for the Healthcare Industry"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium Viscosity Acetal Homopolymer Developed for the Healthcare Industry"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":24086,"state":0,"general":{"pos":2,"name":"Delrin\u00ae PC652 NC010","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2025-08-18 13:58:17","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":10},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for the Healthcare Industry"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for the Healthcare Industry"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":24090,"state":0,"general":{"pos":2,"name":"Delrin\u00ae PC690 NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-08-18 13:58:23","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":8},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":24091,"state":0,"general":{"pos":2,"name":"Delrin\u00ae PC691 NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-02-19 15:42:09","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":10},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":24092,"state":0,"general":{"pos":2,"name":"Delrin\u00ae PC699 NC010","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2025-02-19 15:42:17","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":8},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Silicone Lubricated Low Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for the Healthcare Industry"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Silicone Lubricated Low Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for the Healthcare Industry"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":78723,"state":0,"general":{"pos":2,"name":"Delrin\u00ae RA100CPE NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-12-03 09:17:37","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"High Viscosity Renewable Attributed Acetal Homopolymer with Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"High Viscosity Renewable Attributed Acetal Homopolymer with Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":78724,"state":0,"general":{"pos":2,"name":"Delrin\u00ae RA300CPE NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-06-24 13:31:25","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":2},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium-high Viscosity Renewable Attributed\u00a0Acetal Homopolymer with Improved Processing\u00a0and Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium-high Viscosity Renewable Attributed\u00a0Acetal Homopolymer with Improved Processing\u00a0and Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":78725,"state":0,"general":{"pos":2,"name":"Delrin\u00ae RA500CPE NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-12-03 09:17:37","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium Viscosity Renewable Attributed\u00a0 Acetal Homopolymer with Improved Processing\u00a0and Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium Viscosity Renewable Attributed\u00a0 Acetal Homopolymer with Improved Processing\u00a0and Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":71591,"state":0,"general":{"pos":2,"name":"Delrin\u00ae RA511CPE NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-12-03 09:17:37","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated Medium Viscosity Renewable Attributed Acetal Homopolymer with Very Low Emissions"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated Medium Viscosity Renewable Attributed Acetal Homopolymer with Very Low Emissions"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":79030,"state":0,"general":{"pos":2,"name":"Delrin\u00ae RAFG100 NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-04-15 15:57:05","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"High Viscosity Renewable Attributed Acetal Homopolymer"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"High Viscosity Renewable Attributed Acetal Homopolymer"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":79031,"state":0,"general":{"pos":2,"name":"Delrin\u00ae RAFG500P NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-08-18 14:00:14","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium Viscosity Renewable Attributed Acetal Homopolymer Developed for Food Contact Applications"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium Viscosity Renewable Attributed Acetal Homopolymer Developed for Food Contact Applications"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":79029,"state":0,"general":{"pos":2,"name":"Delrin\u00ae RAFG511DP NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-05-23 13:54:47","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated Medium Viscosity Renewable Attributed Acetal Homopolymer Developed for Food Contact Applications"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated Medium Viscosity Renewable Attributed Acetal Homopolymer Developed for Food Contact Applications"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":79101,"state":0,"general":{"pos":2,"name":"Delrin\u00ae RASC655 NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-08-18 14:00:25","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium Viscosity Renewable Attributed Acetal Homopolymer Developed for the Healthcare Industry"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium Viscosity Renewable Attributed Acetal Homopolymer Developed for the Healthcare Industry"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":79102,"state":0,"general":{"pos":2,"name":"Delrin\u00ae RASC698 NC010","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2025-08-18 13:58:38","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":2},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Silicone Lubricated Low Viscosity Renewable Attributed Acetal Homopolymer with Low Wear and Low Friction Developed for the Healthcare Industry"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Silicone Lubricated Low Viscosity Renewable Attributed Acetal Homopolymer with Low Wear and Low Friction Developed for the Healthcare Industry"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":24084,"state":0,"general":{"pos":2,"name":"Delrin\u00ae SC631 NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2026-03-03 16:23:16","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":8},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Nucleated Medium-high Viscosity Acetal Homopolymer Developed for the Healthcare Industry"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Nucleated Medium-high Viscosity Acetal Homopolymer Developed for the Healthcare Industry"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":1,"eqds":true},{"pos":2,"id":24087,"state":0,"general":{"pos":2,"name":"Delrin\u00ae SC655 NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-08-18 14:00:34","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Medium Viscosity Acetal Homopolymer Developed for the Healthcare Industry"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Medium Viscosity Acetal Homopolymer Developed for the Healthcare Industry"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":24089,"state":0,"general":{"pos":2,"name":"Delrin\u00ae SC690 NC010","abbt":"POM","pname":"","pshortname":"DuPont","lastchange":"2025-08-18 13:58:51","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":0},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":53560,"state":0,"general":{"pos":2,"name":"Delrin\u00ae SC698 NC010","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2025-08-18 13:59:02","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":2},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Silicone Lubricated Low Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for the Healthcare Industry"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Silicone Lubricated Low Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for the Healthcare Industry"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true},{"pos":2,"id":24848,"state":0,"general":{"pos":2,"name":"Delrin\u00ae SC699 NC010","abbt":"POM-Z","pname":"","pshortname":"DuPont","lastchange":"2025-08-18 13:59:12","region":[],"assortment_name":"","assortment_color":"","moisturedep":null,"status":8},"tile":{"description":{"pos":4,"name":"Product Information","content":[{"type":"text","name":"Product Information","content":"Silicone Lubricated Low Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for the Healthcare Industry"}]}},"list":{"description":{"pos":4,"name":"Product Information","content":"Silicone Lubricated Low Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for the Healthcare Industry"}},"table":[],"sortby":0,"applications":[],"injds":1,"psds":false,"bmds":false,"extrds":0,"eqds":true}],"links":{"first":"https:\/\/delrin.materialdatacenter.com\/api\/v1\/material\/products?page=1","last":"https:\/\/delrin.materialdatacenter.com\/api\/v1\/material\/products?page=1","prev":null,"next":null},"meta":{"current_page":1,"from":1,"last_page":1,"path":"https:\/\/delrin.materialdatacenter.com\/api\/v1\/material\/products","per_page":100,"to":93,"total":93}}